Seawater attacks a ship in three distinct ways.
It corrodes the hull and underwater structure electrochemically. It carries marine organisms that colonize sea chests, condensers, and cooling piping. And the electrical plant itself drives stray currents through the shaft line. Each failure mode needs its own countermeasure, so shipbuilders fit three: an impressed current cathodic protection (ICCP) system for the hull, a marine growth prevention system (MGPS) for the seawater side, and a shaft grounding device for the propeller shaft. Together they form the protective barrier around the underwater part of the ship.
ICCP: Active Corrosion Protection for the Hull
Sacrificial anodes versus impressed current
Cathodic protection comes in two forms. The sacrificial anode method connects a more active metal, typically zinc or aluminum, directly to the steel structure. The anode dissolves and supplies protective current to the steel. Ships using this method fit zinc anode blocks along the bilge keel flowline, in sea chests, inside double bottoms and void spaces, and on the rudder and propeller. Aluminum alloy anodes perform better than zinc, but classification rules prohibit them in machinery spaces and cargo oil tanks because their high operating potential can generate sparks. Sacrificial anodes carry a design life of 2 to 3 years and are inspected and renewed as a set at every drydocking.
An ICCP system takes the opposite approach. Instead of consuming metal, it uses external power and long-life anodes to drive protective current, which makes it the active defense layer for the hull.
How ICCP works
Steel immersed in seawater corrodes through anodic oxidation: Fe → Fe²⁺ + 2e⁻. The metal literally dissolves as it loses electrons. An ICCP system counters this by pushing the hull potential negative into the protected range. Hold the steel below -0.85 V against a silver/silver chloride reference electrode (measured in 3.5% sodium chloride solution at 25°C) and the dissolution rate falls below roughly 0.01 mm per year, low enough to ignore over a docking cycle.
The system holds that potential with a closed control loop. Reference electrodes on the hull feed potential readings to the potentiostat, which uses PID control with about ±1% regulation accuracy to trim its output current. If the potential drifts above roughly -0.8 V the hull is under-protected and the system raises the current. If it falls below about -1.1 V the hull is over-protected, which risks paint disbondment and hydrogen embrittlement of the steel, so the system cuts the current back immediately.
Seawater conditions shift the targets. For every 10°C rise in water temperature the protection potential needs to move about 50 mV more negative. When salinity drops by 10 parts per thousand, for example entering an estuary, conductivity falls with it, so current density should be reduced by around 15% to avoid wasting energy.